1. … 25Cr type duplex stainless steels especially for Super Duplex grade, PRE (Pitting Resistance Equivalent) is over 40. Ar-CO2 mixed gas or …
  2. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Mixing arms, Cold cutting tools, Hammers, …
  3. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …
  4. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good …
  5. … and refurbishment is the most common application.Magnesium 92/8 is preferred for joining many casting alloys. … Magnesium alloys, 2L124, …
  6. … metal requires no buffer layer. Suited for wear parts subject to heavy pressure, impact and shock. The interpass temperature should be maximum …
  7. … ER409 alloy. Single pass welds on light gage base metal or welds with preheat do not usually require PWHT. … 1.4000, 1.4002, 1.4016, 1.4057, …
  8. … alloys and covers a huge range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg4,5Mn, …
  9. … and cleaning method during production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding …
  10. … properties than Grade 2 or 3 and is sometimes specified for pressure vessels or piping for its superior strength alone. … Titanium …