1. … very stable, spatter free arcs. This wire deposits low carbon weld metal of about 23%Cr-13%Ni-2.3%Mo. Cladding on low alloyed steels,the weld metal already achieves approximately the composition of ASTM 316 in the …
  2. … 10 times faster than overlay welding by SMAW. No dilution with the basemetal and a full high hardness in the total thickness of the plate. No excessive heat that effects the basemetal or cause loose in strength two times faster to apply compare to …
  3. … Outstanding alloy against high impact combined with abrasion including metal into metal friction. The weld deposit of CEWELD E Dur 60 Kb is one of the …
  4. … °C and the deposition rate is 20-30% higher than with comparable tube metal. It is easy to use and inexperienced welders will have no … matters. Use a larger tip than is generally recommended for same diameter mild steel. Use slight excess acetylene feather. The deposit is …
  5. … Fully austenitic weld metal with high resistance against stress corrosion cracking and … Ni, Mo and Cu. Sufficient resistance against oxidizing acids. The weld metal is corrosion resistant in sea water. CEWELD® SA Alloy 825 is best …
  6. … suitable for MIG welding, easy to handle, high plasticity of the weld metal. High quality alloyed copper wire. The weld metal is a Copper-Silver alloy. Sound, pore free deposits and high …
  7. … carbon maintains a low level of free carbon and enables the filler metal to be used with Nickel 201. The weld metal has good corrosion resistance, particularly in alkali’s.  … … for surfacing of steel. Dissimilar welding applications of filler metal NiTi 3 include joining Nickel 200 and 201 to stainless steels, …
  8. … interpass temperature and post weld treatment as required for the base metal. Hydrogen content: HD < 3 ml / 100 g weld metal. CEWELD E 11018-H is packed in the best in class multi layer …
  9. … water, liquid acids, flue gas, corrosive gas.Low friction properties (metal to metal wear) … Copper aluminum metal spray wire for sea water resistant coatings, bearings, treads …
  10. … temperatures (500-800°C) under long term creep conditions. This filler metal can also be used for welding 321/321H and 347/347H grades in high … by intergranular HAZ cracking is reduced by using more ductile weld metal rather than 347H. … ISO 15608: 8.1  Austenitic ≤ 19 % Cr , TÜV …