1. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast … EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350, GG10, GG15; GG20, GG25; GG30; GG35; GG40 EN 1562: EN-GJMB-350, EN-GJMB-550 , EN- GJMW-350, EN- GJMW-550 , GTS 35, GTS 55, GTW 35, …
  2. … wires. Excellent weld metal quality. Operating temperatures up to +350 °C. CEWELD AA 4361 is primarily used in flat and horizontal …
  3. … in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing peddles, …
  4. … alloy containing Nickel for more strength and bridging capability during brazing with excellent rebuilding properties.  Flux/Paste: …
  5. … Kaiserslautern   Handelsregisternummer  HRB 32815 Vertreten durch Herrn Martin Adam Grzeganek                            Kontakt: …
  6. … that this steel is distinctly vulnerable to sensitization phenomenon during welding, even though martensite hogs a great amount of carbon …
  7. … for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to … ISO 15608: 8.1  Austenit ≤ 19 % Cr 9%Ni ,TÜV 1000: Gr. 21 - 22 (29 max.350°C), 1.4301, 1,4306, 1.4307, 1.4308, 1.4311, 1.4312, 1.6900, 1.6901, …
  8. … and leaves a fine rippled shiny surface. Max. service temperature 350ºC. Corrosion resistance similar to low carbon CrNiMo(Mn,N)-steels. …
  9. … For the best results, welding must be done in a low heat input procedure and is not recommended for multi-pass applications … 1.4512,  …
  10. … resistance to intercrystallin corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon CrNiMo …