1. … alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. … Aircraft gas …
  2. … required as alloys of such chemistry are sensitive to embrittlement at 600-800 °C. The interpass temperature should not exceed 300 °C. … … G-X40CrNiSi 27 4, AISI 327, 442, 446, ASTM A 297 HC UNS S44200, 44600, J92605, J93005, J92605  … 1.4820 … 4820 AC … 3581-A: E 25 4 R 32 …
  3. … oxidation, at service temperatures ranging from 1200°F (650°C) up to 1600°F (870°C) … AMS 5708, 5709, 5706, 5707, 5704, 5544, 5586. PWA 1005, …
  4. … alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. … Aircraft gas …
  5. … innovativer Schweißprozesse und -verfahren zu schaffen. Der Standort (600 m2) bietet Platz für die hochwertigsten und innovativsten …
  6. … of the weld deposit will degrease 16% at 300°C and about 30% at 600°C. Excellent alloy against thermal shock, abrasion, erosion, …
  7. … developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good resistance to general …
  8. … and by grinding. The hardness of the weld deposit will degrees 20% at 600°C and has a nominal hardness of 49-53 HRc at room temperature. The …
  9. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel … Alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … 2.4665 … Alloy X … A 5.14: ERNiCrMo-2 … 18274: S Ni 6002(NiCr21Fe18Mo9) …
  10. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600°F (650, 760 and 870°C) for 16,000 hours. Suitable for joining and … alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … 2.4665 … Alloy X Tig … A 5.14: ERNiCrMo-2 … 18274: S Ni …