1. … Mo content, with low carbon content (less than 0.05%), to be used for welding creep resistant steels. … For 2.5%Cr-1%Mo-alloyed, …
  2. … A continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% …
  3. … Basic electrode with excellent welding characteristics,  Hydrogen content HD < 3 ml/100 g. Meets NACE …
  4. … productivity and weldability, better wetting compared to solid wires.Excellent weld metal quality and X-ray soundness and excellent …
  5. … A Rutile basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% …
  6. … deposits are air-hardenable that can normally be heat-treated after welding. … 1.4000, 1.4001, 1.4002, 1.4003, 1.4006, 1.4008,  1.4021, …
  7. … improved de-oxidation and strength, excellent wetting for increased welding speed with corresponding flux.  Suitable fluxes are depending …
  8. … improved weldability, better wetting properties compared to solid wires. Excellent weld metal quality. Operating temperatures up to +350 …
  9. … Applicable for welding of joints and surfacings of stabilized, corrosion resistant …
  10. … manganese steels. Very good weld deposit appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … …