1. … processing of high-strength, low temperature fine-grained structural steels with Rp0,2 > 500 MPa. Low hydrogen content HD< 3 ml/100g even …
  2. … CEWELD® E 9016-B9 is designed to weld equivalent ‘type T91’ T92 CrMo steels modified with small additions of Tungsten and Vanadium to give …
  3. … spatter loss, easy slag removal. Well suited for joining high carbon steels and when welding critical mixed base metal combinations. Ideal …
  4. … solutions (a form of degradation to which the austenitic stainless steels are prone). It is able to withstand a wide range of oxidizing …
  5. … is a bronzed wire to offer excellent feeding properties with standard steel liners. … S185-E360, S235JR-S355JR, S235J0-S450J0, S235J2-S355J2, …
  6. … Higher corrosion resistance then standard Duplex steels with also higher mechanical properties due to the addition of Nitrogen. … Welding wrought, forged or cast super duplex stainless steels for service in the as-welded Condition. Heterogeneous welding between super duplex stainless steels and dissimilar welds between other stainless and mild or low …
  7. … TIG/GTAW rod for T24 creep resistant steel. The T24 alloy is a modified 2.25%Cr1%Mo alloy with additions of … max. 300°C … alloy 24, 2.5%Cr1%Mo modified, creep resisting ferritic steels. X7CrMoVTiB 10-10 1.7378 / 7CrWVMoNb9-6 - 1.8201 ASTM: A/SA 335 …
  8. … welding. It can be used on a variety of austenitic and ferritic steels and nickel alloys. … Mat No :1.4859, 1.4861, 1.4876, 1.4877, …
  9. … alloyed submerged arc welding wire for offshore requirements upto S460 steels that have to fullfill impact requirements down to -60 degrees … flux or with FL CS155 fused flux. … Materials shipbuilding Unalloyed steels boiler steels pipe steels - Fine grain steels API-standard DIN A, B, D, E, AH …
  10. … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. AA 310B has good general oxidation …