1. … This alloy offers excelent weldabillity when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good … 3.3315, 3.3535, 3.3206, 3.3541, EN AW 5005A, EN AW 5754, EN AW 6060, EN AC 51100, EN AW 5454, EN AW 5251 … AlMg 3 Tig … A 5.10: ER5754 …
  2. … High pressure resistance and high wear resistance. The alloy is characterized by very low thermal electromotive force (emf) compared to …
  3. … NiCrMo 686 (UNS N06686/W.Nr. 2.4606) is a single-phase, austenitic … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected … and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and INCONEL alloys 622, C22, 625, …
  4. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  5. … Very good abrasion resistance in combination with impact even at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …
  6. CEWELD AquaForce MG offers a high deposition rate with remarkable … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO 15608: 1.1, 1.2 1.0035, 1.0570, 1.0461,1.0562, …
  7. … Excellent weldabillity and good mechanical strength combined with good … alloys and covers a huge range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg4,5Mn, … 3.3211, 3.4335, EN AW 5086, EN AW 5083, EN AW 5019, EN AW 5019, EN AW 6060, EN AW 6005A, EN AW 6082, EN AW 6061, EN AW 7020, EN AC 51300, EN …
  8. … De nombreuses années d'essais de nouvelles compositions de rechargement ont permis d'obtenir un nouveau fil de soudure spécial pour Nihard, d'une durée de vie exceptionnelle Après 1547 heures …
  9. … Submerged arc welding wire for welding fine grain steels for low temperature requirements down to -60°C in apparatus, construction and offshore applications. …   … 19Mn5 St 35.8, St 45.8 StE 210.7 TM, StE 480.7 TM StE 255 to StE 460 X 42, X65, X 70 EN same S185 - S355-S460 P235GH, P355GH P235T1/T2, …
  10. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Stone …