1. … thermal shock resistance and impact values at sub zero temperatures down to -196 °C … Dissimilar welds for which the electrode are used …
  2. … MPa. Crack resistant and well suited for low-temperatures, ductility down to -50°C. Preheating, interpass temperature and post weld …
  3. … welding characteristics. High impact strength at sub zero temperatures down to -60 °C. …   Reh < 690 MPa Iso 15608: 3.2 ( 460 < Reh ≤ 690 MPa) …
  4. … with more deposit) No slag losses compare to 40% loss with standard electrodes.! Low amperage offers much lower heat input! 6 mm is ideal …
  5. … excellent all-position welding with higher currents. Applicable down to -40°C. Low spatter loss and remarkably easy slag removal. Due …
  6. … on metallurgical chemistry and excellent subzero impact properties down to -60°C. … Materials shipbuilding Unalloyed steels boiler steels …
  7. … purity, superior hot cracking and corrosion resistance. CVN toughness down to –120 °C, resistant to intergranular corrosion up to 400 °C. …
  8. … weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  9. … as wetting and reduce of spatter.  Excellent for use in position and down hand as well. The fast freezing slag unables CEWELD® AA 308LP to …
  10. … otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …