1. … weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  2. … purity, superior hot cracking and corrosion resistance. CVN toughness down to –120 °C, resistant to intergranular corrosion up to 400 °C. …
  3. … manual and (semi- and fully) mechanized welding. Good quality values down to -40°C. Low spatter losses with excellent slag removability. …
  4. … High strength weld deposit with good impact properties down to -60°C. S3 NiMo1 can be used in combination with FL 851 and FL …
  5. … a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  6. … Suitable for downhand butt- and fillet weld, smooth welding pool without spatter …
  7. … all positional pipe welding electrode designed especially for vertical down root pass welding on DC- and for subsequent passes on DC+. Apart …
  8. … soundness and excellent slag removal.Excellent for use in position and down hand as well. High resistance against moisture pick up.  … ISO …
  9. … HR can be used in all positions, especially suitable for vertical down (PG) position. … Reh ≤420 MPa (60 ksi) ISO 15608: 1.1, 1.2 1.0035, …
  10. … amazingly fast freezing and therefore especially preferred in vertical down position with high speed and deep penetration. Due to the wood …