1. … The Welding Solution Center (WSC) is located at the Agro Park in Huissen and is part of … of new, innovative welding processes and procedures. The location (600 m2) accommodates the highest quality and innovative welding … offer your company, click here . Together with our partners we will present a number of issues during the year and we offer you the …
  2. … As earlier announced the new standard according EN ISO 1090 has entered the market  from the first of July … DNV, TUV, etc. of course our team is ready to support you with your pre-WPS and also with physical support and guidance during welding. … …
  3. … Alloy C276 is a popular nickel-molybdenum-chromium alloy renowned for its … corrosion-resistant weld.   Typical chemical composition in % Ni: 50-60 Cr: 14.5-16.5 Mo: 15-17 Fe: 4-7 W: 3-4.5 Co: ≤ 2.5 Mn: ≤ 1 Small … use in oil and gas processing environments where hydrogen sulfide is present. Alloy C276 is widely used in industries such as chemical …
  4. … Alloy 625 has high resistance to corrosion in both acidic and alkaline environments. It exhibits … encountered in chloride-containing environments. Alloy 625 finds widespread applications in industries such as chemical processing, …
  5. … Alloy 600 is a nickel-chromium alloy with good corrosion resistance to a wide range of … high temperatures and corrosion resistance. When welding Alloy 600, CEWELD® NiCro 600 can be used as filler material. This ensures … stress corrosion cracking, a type of corrosion that occurs in the presence of chlorides at elevated temperatures. Water Corrosion: Alloy …
  6. … These alloys are specially designed for high-temperature applications. They offer … chemical composition in % Ni: 30-35 Cr: 19-23 Fe: 39.5-42.5 Al: 0.15-0.60 Ti: 0.15-0.60 C: ≤ 0.10 Cu: ≤ 0.75 Small amounts of other elements … it suitable for applications in industries where sulfur compounds are present. Chloride-Ion Stress Corrosion Cracking (SCC) Resistance: Alloy …
  7. … usually under supervision of DNV , Lloyds , Bureau Veritas  and ABS because they have created a set of rules with minimum requirements to grand safety in the construction. In general, these rules are pretty much the same but require lots of experience to meet in …
  8. CEWELD E FeNi 60 N has a few benefits compare to other “FeNi” types … current, non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you … EN-GJS-400-15, EN-GJS-400-18, EN-GJS-450-10, EN-GJS-500-7, EN-GJS-600-3, EN-GJS-700-2. GGG40, GGG45, GGG50, GGG60; GGG70, GGG80 … E FeNi …
  9. … point and narrow freezing range. In addition, it has a higher silicon content than AlSi5, which provides increased fluidity and reduced … elevated temperatures. Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11, G-AlSi12 …
  10. … Hardfacing alloy for cladding steel mill rollers, thermoshock resistant and suitable for Francis and Pelton turbines. Used in … hardness and is resistant against metal-metal wear and high surface pressure.  … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …