1. CEWELD E DUR 25U is a Cobalt based electrode developed to resist high impact load, high heat, thermal shock, hot corrosion, compression, abrasion, erosion and many other forms of attack. The weld …
  2. … This pure aluminum filler metal offers excellent weldability when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150 °C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., …
  3. CEWELD® AA 2594 is a flux cored wire designed for welding 25Cr type duplex stainless steels especially for Super Duplex grade, PRE (Pitting Resistance Equivalent) is over 40. Ar-CO2 mixed gas or … UNS S32520, S32550, S32750, S39274, S39277, S39553, S32760, J93380 Ferralium 255, SAF 2507, ZERON 100, UR 76 N, SM22Cr, SAF …
  4. CEWELD® E 6013 S is a medium thick coated electrode for all kinds of … suited for welding jobs at poorly accessible points and badly prepared seams. CEWELD® E 6013 S can be sued in all positions, in particular it is ideally suited …
  5. CEWELD® MA 600 (1.4718) offers outstanding abrasion resistance combined … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. … 600 HB, T Fe 8 … MA 600 (1.4718) … A 5.21: ERFeCr-A … 14700: T Fe8 …
  6. … This alloy offers excellent weldability when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good … 3.3315, 3.3535, 3.3206, 3.3541, EN AW 5005A, EN AW 5754, EN AW 6060, EN AC 51100, EN AW 5454, EN AW 5251,   … AlMg 3 … A 5.10: ER5754 …
  7. … Zirconium often is chosen for its resistance to corrosion from most … subsequent passes until the root surface temperature stays below 600 degrees F. Backup shielding also should be used on the back surface of sheet or plate less than 1/4 in. thick to prevent oxidation. Gas Requirements. Welding-grade argon (99.999 …
  8. … Ductile welding deposit with high conductivity and corrosion resistance. … as most commercial copper grades. Thicker sections than 5 mm should be preheated up to approximately 500 °C. … Cladding steel, Grey cast iron, … Copper, Copper Alloys and dissimilar welding.  Mat.n: 2.0040, 2.0060, 2.0070, 2.0076, 2.0080, 2.0090, 20100, 2.0110, 2.0150, 2.0170  UNS: …
  9. … This pure aluminum filler metal offers excellent weldability when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  10. … Due to the high resistance to cracking and toughness, all weld metal requires no buffer layer. Suited for wear parts subject to heavy pressure, impact and shock. The interpass temperature should be maximum …