1. … MPa. Crack resistant and well suited for low-temperatures, ductility down to -50°C. Preheating, interpass temperature and post weld …
  2. … on metallurgical chemistry and excellent subzero impact properties down to -60°C. … Materials shipbuilding Unalloyed steels boiler steels …
  3. … welding characteristics. High impact strength at sub zero temperatures down to -60 °C. Weldable with Co2 and Mixed gas. … Reh < 690 MPa Iso …
  4. … weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  5. … welding of pipes with a yield strength up to 500 MPa and impact energy down to -40°C. Due to its alloying concept (even with < 1%Ni) it is …
  6. … excellent all-position welding with higher currents. Applicable down to -40°C. Low spatter loss and remarkably easy slag removal. Due …
  7. … CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to nitric acid. … ISO 15608: 8.1 …
  8. … otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  9. … flux cored wire for extreme requirements at sub zero temperatures down to -60 °C. Excellent welding properties.  Yield strength < 600 …
  10. … as wetting and reduce of spatter.  Excellent for use in position and down hand as well. The fast freezing slag unables CEWELD® AA 308LP to …